Controlling solid electrolyte interphase (SEI) in batteries is crucial for their efficient cycling. Herein, we demonstrate an approach to enable robust battery performance that does not rely on high fractions of fluorinated species in electrolytes, thus substantially decreasing the environmental footprint and cost of high-energy batteries. In this approach, we use very low fractions of readily reducible fluorinated cations in electrolyte (∼0.1 wt%) and employ electrostatic attraction to generate a substantial population of these cations at the anode surface. As a result, we can form a robust fluorine-rich SEI that allows for dendrite-free deposition of dense Li and stable cycling of Li-metal full cells with high-voltage cathodes. Our approach represents a general strategy for delivering desired chemical species to battery anodes through electrostatic attraction while using minute amounts of additive.
| שפה מקורית | אנגלית |
|---|---|
| עמודים (מ-עד) | 4137-4146 |
| מספר עמודים | 10 |
| כתב עת | Energy and Environmental Science |
| כרך | 17 |
| מספר גיליון | 12 |
| מזהי עצם דיגיטלי (DOIs) | |
| סטטוס פרסום | פורסם - 2 מאי 2024 |
טביעת אצבע
להלן מוצגים תחומי המחקר של הפרסום 'Robust battery interphases from dilute fluorinated cations'. יחד הם יוצרים טביעת אצבע ייחודית.פורמט ציטוט ביבליוגרפי
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver