דילוג לניווט ראשי דילוג לחיפוש דילוג לתוכן הראשי

IR laser power transmission through silver halide crystals and polycrystalline fibers

  • Lev Nagli
  • , D. Burstein
  • , Shaul Shalem
  • , David Bunimovich
  • , Alla German
  • , Abraham Katzir

פרסום מחקרי: פרסום בכתב עתמאמר מכנסביקורת עמיתים

תקציר

Laser-induced breakdown (LIB) thresholds in AgClxBr 1-x crystals and fibers were studied under CO2 laser pulses and CW excitation. The value of LIB threshold Pc of the bulk crystals is about 7.2·108 W/cm2 for AgCl and 4·109 W/cm2 for AgBr under 60 ns TEA laser excitation. The LIB threshold in fibers is much smaller; about 2·10 8 W/cm2. The absorption of the crystals at 10.6 μm changes from 8·10-5 cm-1 for AgCl to 2·10-5 cm-1 for AgBr; for fibers with the same composition absorption is much greater (3·10-4 cm-1 for AgCl; 2·10-4 cm-1 for AgBr). The dependence of the LIB and IR absorption on composition, and mechanical and temperature treatments suggests that the LIB in silver halide crystals and fibers is due to the avalanche electrons in a high electric field. The initial free electrons for this process are supplied by ionization of the cation vacancy - charged dislocation complexes. The relatively lower optical stability of the fibers is due to the increased concentration of defects formed in the hot extrusion of the crystal. A simple thermal annealing method for reduction of the IR absorption is proposed.

שפה מקוריתאנגלית
עמודים (מ-עד)545-552
מספר עמודים8
כתב עתProceedings of SPIE - The International Society for Optical Engineering
כרך2966
מזהי עצם דיגיטלי (DOIs)
סטטוס פרסוםפורסם - 1997
פורסם באופן חיצוניכן
אירועLaser-Induced Damage in Optical Materials: 1996 - Boulder, CO, ארצות הברית
משך הזמן: 7 אוק׳ 19967 אוק׳ 1996

טביעת אצבע

להלן מוצגים תחומי המחקר של הפרסום 'IR laser power transmission through silver halide crystals and polycrystalline fibers'. יחד הם יוצרים טביעת אצבע ייחודית.

פורמט ציטוט ביבליוגרפי